  • ABS Grade AH32 steel plate,ABS Grade AH36 shipbuilding plate
  • ABS Grade D steel plate,ABS Grade E shipbuilding plate
  • ABS Grade A steel plate,ABS Grade B shipbuilding plate
  • SMA570W SMA570P weathering steel plate
  • SMA490AP SMA490BP SMA490CP weathering steel plate
  • SMA490AW SMA490BW SMA490CW weathering steel plate
  • SMA400AP SMA400BP SMA400CP weathering steel plate
  • SMA400AW SMA400BW SMA400CW weathering steel plate

  •  Accreditation Administration System:
  • Home-Technology

    Technology

  • Adopting standard: LR DH36
  • Shipbuilding steel plates LR DH36 with minus 20 centidegree impacting test in rolling.

    Please see more date in Chemical composition and mechnical property as below:

    Adopting standard: LR

    Relative Grades:LR A|LR B|LR D|LR E|LR AH32|LR AH36|LR AH40|LR DH32|LR DH36|LR DH40

    |LR EH32|LR EH36|LR EH40|LR FH32|LR FH36|LR FH40

    Property Data:

                                            LR

    Grade

    T: 8-300MM

    LR AH36

    LR DH36

    LR EH36

    LR FH36

    Chemical 

    Composition

     %  ≤

    C

    0.18

    0.16

    Mn

    0.9-1.60

    P

    0.035

    0.025

    S

    0.035

    0.025

    Si

    0.50

      Al (acid)

    ≥ 0.015

    Nb

    0.02-0.05

    V

    0.03-0.10

    Ti

    0.02

    Ni

    0.40

    0.80

    Cu

    0.35

    Cr

    0.20

    Mo

    0.08

    N

    0.009

    Mechanical

     Property ≥

    Yield Strength

    (Mpa)

    355

    355

    355

    355

    Tensile Strength

    (Mpa)

    490-620

    490-620

    490-620

    490-620

    Impacting Test 

    temperature (℃)

    0

    -20

    -40

    -60

    Mark

    LR/A36

    LR/D36

    LR/E36

    LR/F36

    H:Heat Analysis.   P:Product Analysis

    NOTE:As for Grade LR DH36 plates,if the thickness above 12.5mm,the delivery condition

    must be Normalized or Normalized rolled or TMCP.As rolled is not allowed to delivery 

    without the customer’s special requirement.

    For more technical data,please link:

     

     

    Shipbuilding plate    Boiler plate    Offshore platform plate    High strength plate    Low alloy plate    Pipeline plate    Carbon plate    Shipbuidling profiles    
  • YUSHENG IRON AND STEEL CO.,LIMITED, All Rights Reserved.
  • T:0086-371-23846710 WhatsApp:0086-13526581176 E-mail:admin@ysteelplate.com
  • Add:East Area,25thFloor,Y.H.International Plaza,Zhengzhou City,Henan province in China. A516Gr70|P355GH We can offer:P355GH,ABS EH36,A516Gr70,A131GrA,S690Q,A572Gr50,API X60,A283GrC,LR AH36,ABS AH32,LR DH36.etc.