DNV Grade AH36 and EH36
Shipbuilding steel plates DNV Grade AH36 shall be normally used to build the vessel body,and DNV Grade EH36
shall be mainly used to build heavy crane of vessels.Generally we also would provide our customers Z test
including Z15,Z25,Z35 on these plates for providing the property.
Relative Grades:DNV A|DNV B|DNV D|DNV E|DNV AH32|DNV AH36|DNV AH40|DNV DH32|DNV DH36|
DNV DH40|DNV EH32|DNV EH36|DNV EH40|DNV FH32|DNV FH36|DNV FH40
Please find the chemical composition and tensile strength deatails of DNV Grades AH36,DH36,EH36 and FH36.
Property Data:
DNV | ||||||
Grade |
T: 8-300MM |
DNV AH36 |
DNV DH36 |
DNV EH36 |
DNV FH36 | |
Chemical Composition % ¡Ü |
C |
0.18 |
0.16 | |||
Mn |
0.9-1.60 | |||||
P |
0.035 |
0.025 | ||||
S |
0.035 |
0.025 | ||||
Si |
0.50 | |||||
Al (acid) |
¡Ý 0.015 | |||||
Nb |
0.02-0.05 | |||||
V |
0.03-0.10 | |||||
Ti |
0.02 | |||||
Ni |
0.40 |
0.80 | ||||
Cu |
0.35 | |||||
Cr |
0.20 | |||||
Mo |
0.08 | |||||
N |
|
0.009 | ||||
Mechanical Property ¡Ý |
Yield Strength (Mpa) |
355 |
355 |
355 |
355 | |
Tensile Strength (Mpa) |
490-620 |
490-620 |
490-620 |
490-620 | ||
Impacting Test temperature (¡æ) |
|
0 |
-20 |
-40 |
-60 | |
Mark |
|
NV/AH36 |
NV/DH36 |
NV/EH36 |
NV/FH36 |
H:Heat Analysis. P:Product Analysis