TMCP and Normalized shipbuilding steel plates ABS FH32,ABS FH36 and ABS FH40 under ABS calssification
society approved. These steel grades would be done the special lowest temperature impacting test at_60
centidegree.Owning to this special requirement,these steel grades mainly be used to building breakers which
work in the lowest surroundings.Else,FH class steel plates still have some difference in Chemical composition
with other high strength shipbuilding steel grades.Please foucs on the following table to check.
Property Data:
ABS | ||||||
Grade |
|
ABS FH32 |
ABS FH36 |
ABS FH40 | ||
Chemical Composition % ¡Ü |
C |
0.16 | ||||
Mn |
0.90-1.60 | |||||
Si |
0.10-0.50 | |||||
P |
0.025 | |||||
S |
0.025 | |||||
Al (acid) |
0.015 | |||||
Nb |
0.02-0.05 | |||||
V |
0.05-0.10 | |||||
Ti |
0.02 | |||||
Cu |
0.35 | |||||
Cr |
0.20 | |||||
Ni |
0.80 | |||||
Mo |
0.08 | |||||
N |
- | |||||
Mechanical Property ¡Ý |
Yield Strength (Mpa) |
315 |
355 |
390 | ||
Tensile Strength (Mpa) |
440-590 |
490-620 |
510-650 | |||
Mark |
|
AB/FH32 |
AB/FH36 |
AB/FH40 |