Adopting standard: ASTM / ASME
Relative Grades:ASTM A285GrA|A285GrB|A285GrC|ASME SA285GrA|SA285GrB|SA285GrC
Property Data:
|
ASTM | ||||
|
Grade |
T: 8-350MM |
A285GrA |
A285GrB |
A285GrC |
|
Chemical Composition % ¡Ü |
C |
0.17 |
0.22 |
0.28 |
|
Mn H |
0.90 |
0.90 |
0.90 | |
|
P |
0.98 |
0.98 |
0.98 | |
|
P |
0.035 |
0.035 |
0.035 | |
|
S |
0.035 |
0.035 |
0.035 | |
|
Mechanical Property ¡Ý |
Yield Strength (Mpa) |
165 |
185 |
205 |
|
Tensile Strength (Mpa) |
310-450 |
345-485 |
380-515 | |
H:Heat Analysis. P:Product Analysis